Let's learn about measures to reduce and prevent the formation of oxide scale today. For the flame heating furnace, according to the heating environment factors that affect the formation of oxide scale, corresponding measures can be taken in the heating process to achieve the purpose of reducing the formation of oxide scale. The main measures are as follows:
O'rtacha himoya isitish. Pishiriqni qizdirilganda oksidlanishiga yo'l qo'ymaslik uchun uning yuzasini oksidlovchi o'choq gazidan ajratib oling. Ishlatilgan muhitlarga gazsimon himoya vositalari (masalan, toza gaz, suyultirilgan neft gazi, azot va boshqalar), suyuq muhit (shisha eritmasi, erigan tuz va boshqalar) va qattiq himoya vositalari (ko'mir, shisha kukuni, emal kabi) kiradi. kukun va metall qoplamasi Kutib turing).
Let's learn more about the hazards of oxide skin. Oxide scale will cause a large amount of loss of metal materials: The oxide scale generated when metal is heated causes a large amount of loss of metal materials. In general, {{0}}.5 percent to 3.0 percent of the metal is burned out every time the billet is heated. In severe cases, the burn rate can even reach 5 percent
Biz bilan zhang@pride-cnc.com manzili orqali bog‘laning